Important! Please do not add any air when stirring the paint as this is included in the paint film depending on the drying conditions. This would lead to an impairment of the surface and the load-bearing capacity of the coating.

TEMAFLOOR  P 300

DESCRIPTION    
A two component, solvent free epoxy coating.

PRODUCT FEATURES
   

For new and old concrete floors exposed to heavy mechanical and chemical stress in industrial and storage facilities, repair shops; e.g. process or paper machine units and corridors.

RECOMMENDED USES      Finncoatings®color on the highest level 
Also suitable for car parks, garages, business premises, shopping centres, restaurants and cafe`s.

TECHNICAL DATA   Finncoatings®color on the highest level

Features    
Good resistance to abrasion. Withstands water, oils, greases, chemicals and dilute solutions of non-oxidizing acids, alkali and salt solutions. Resists only temporary splashes of oxidizing acids and bleaching chemicals. A separate chemical resistance table available. Withstands +70ºC dry heat and +60ºC in immersion. Does not resist abrupt, great or repeated changes of temperature. Self-levelling. Temafloor Flex hardener makes the paint surface flexible and thus more resistant to cracking of concrete. Also RAL EFFECT metallic colour shades available. Fire classification: Fire classification according to standard EN 13501-1 is BFL-s1.

Colour Cards
   
RAL, NCS, SSG, BS, MONICOLOR NOVA and SYMPHONY colour cards. TEMASPEED tinting. Also metallic shades are available.

Gloss groups
       Finncoatings®color on the highest level
Full-gloss

Coverage     
Coverage on concrete floors is on the average:
Film thickness 0.3 mm coverage approx. 3 m2/litre
Film thickness 0.5 mm coverage approx. 2 m2/litre

 
Practical coverage depends on the porosity and evenness of the substrate and on the application method.
Mixing ratio     Base 4 parts by volume 167 serie
Hardener 1 part by volume 008 4514

or

Paint 2 parts by volume 167 serie
Flex hardener 1 part by volume 930 5002
Application method     Pour the coating mixture onto the floor and spread it with a serrated steel trowel or a trowel. Level with a roller.
Pot-life (+23°C)     20 - 30 minutes on substrate, approx. 15 minutes in the mixing container.
Drying time at 23°C and 50% relative air humidity     

Dust dry after 6 hours
Light trucking after 16 hours
Fully cured after 7 days   Finncoatings®color on the highest level

At lower temperature the curing process will last longer.
With Temafloor Flex hardener the curing times are a little longer than with standard hardener.

Solids volume
    Approx. 100 %.
Density     1.4 kg / litre (mixture)

APPLICATION DETAILS

Application conditions    
The relative humidity of the concrete should not exceed 97%. The temperature of the ambient air, surface or coating should not fall below + 15ºC during application or drying. Relative humidity of air should not exceed 80%.
Note! There is a natural tendency of epoxy coatings to chalk and discolor on exterior exposure.

Preparation
   

New concrete   Finncoatings®color on the highest level
Remove laitance by power grinding, vacuum grit blasting or hydrochloric acid etching. Choose the method best suited for the premises. After grinding remove dust carefully with a vacuum cleaner. Hydrochloric acid etching is carried out with diluted hydrochloric acid
(1 part concentrated hydrochloric acid, 4 parts water). Rinse with plenty of water. Dry the floor.

Old concrete
Remove all grease, oil, chemicals and other impurities by MAALIPESU detergent. Remove old peeling paint layer by grinding or vacuum grit blasting. Choose the method best suited for the premises. Clean out pot-holes removing all loose friable material. Open cracks with e.g. an abrasive tool. Remove loose material and dust.

Cementitious levelling screed
Check compatibility with the levelling screed manufacturer.

Priming
       Finncoatings®color on the highest level
Prime using 30–50% with Thinner 1029 (or 1031) thinned Temafloor 200 Primer or 400 epoxy varnish. Pour the varnish mixture onto the floor and apply as much as is needed to impregnate the concrete surface. If necessary, repeat priming to get a non-porous surface. Subsequent treatment can be carried out after 2 hours using "wet-on-wet" technique. A porous priming coat will result in holes and air bubbles in the finished screed.
Patching     Patch pot-holes and cracks with Colofill putty or a mixture of unthinned Temafloor 200 Primer epoxy varnish or Temafloor P 300 epoxy coating and dry, clean sand. Mixing ratio e.g. 1 part by volume of epoxy mixture and 1–2 parts by volume of sand of grain size 0.1–0.6 mm. Grind the patched areas before overcoating.
Diluting     Do not thin Temafloor P 300 epoxy coating.
Coating     Overcoating may be carried out with unthinned Temafloor P300 not earlier than 6 hrs and not later than 24 hrs after priming and patching. If the primed surface is not overcoated within 24 hrs, it should be abraded. Pour the coating mixture onto the floor and spread it with a serrated steel trowel or a trowel. Level with a roller. Recommended film thickness is 0.3–0.5 mm.

Mixing of components
       Finncoatings®color on the highest level
Mix the correct proportions of base and hardener thoroughly (approx. 2 minutes) by using a low speed hand drill with a paddle. The amount of mixture depends on the area to be coated and on the pot life of the mixture. Insufficient mixing or incorrect mixing ratio will result in uneven drying of the surface, weaken the properties of the coating and risk the success of the application.

Cleaning of tools    
Thinner 006 1029 or Thinner 006 1031.

EU VOC 2004/42/EC-limit value     VOC 2004/42/EC (cat A/j) 500 g/l (2010)Temafloor P 300: max. VOC < 500 g/l

Finncoatings® Color on the highest level

Finncoatings  
Heidelberger Straße 8
74858 Aglasterhausen-Germany

 

Tel. + 49 (0)6262 917095
Fax  + 49 (0)6262 917791

www.finncoatings.com
Mail. This email address is being protected from spambots. You need JavaScript enabled to view it.