Finncoatings® Color on the highest level

 

Important! Please do not add any air when stirring the paint as this is included in the paint film depending on the drying conditions. This would lead to an impairment of the surface and the load-bearing capacity of the coating.

TEMAFLOOR  PU-UV

DESCRIPTION    
A high solids, elastic two-component polyurethane coating.

PRODUCT FEATURES
       Finncoatings®color on the highest level
Intended as a UV-resistant topcoat on Temafloor PU floors in parking decks and other areas exposed to direct sunlight.
RECOMMENDED USES    
Concreet floors.

TECHNICAL DATA   Finncoatings®color on the highest level

Features    
Withstands medium mechanical and chemical stress. Good impact resistance. Self-levelling, to be applied with serrated or steel trowel.

Colour Range
   
TVT 0229. The shade and gloss of the coating may change during time.

Gloss groups
       Finncoatings®color on the highest level
Gloss

Coverage     
Practical coverage depends on the porosity and evenness of the substrate and on the application method.
Film thickness 0.3 mm coverage approx. 2.7 m2/litre
Film thickness 0.5 mm coverage approx. 1.8 m2/litre
Mixing ratio     Base 2 parts by volume 473 serie
Hardener 1 part by volume 008 4001

Application method        Finncoatings®color on the highest level
Serrated or steel trowel.

Pot-life (+23°C)     40 minutes on substrate, abt. 20 minutes in the mixing container.
Drying time at 23°C and 50% relative air humidity     

Dust dry after 6 hours
Light trucking after 24 hours
Fully cured after 7 days   Finncoatings®color on the highest level

At lower temperatures the curing process will last longer.

Solids volume
   

Approx. 90 % volume
Density     1.4 kg / litre (mixture)

APPLICATION DETAILS

Application conditions        Finncoatings®color on the highest level
The relative humidity of the concrete should not exceed 97%. The temperature of the ambient air, surface or coating should not fall below +15ºC during application or drying. Relative humidity of air should not exceed 70%.
Preparation     Remove dust and loose particles from the floor. Remove all grease, oil and other impurities by detergent washing.
Diluting     Do not thin Temafloor PU-UV polyurethane coating.
Coating     Overcoating may be carried out not earlier than 24 hrs after coating with Temafloor PU. If the coated surface is older than 7 days, it should be abraded. Pour the coating mixture onto the floor and spread it with a serrated steel trowel or an adjustable trowel. Control that the thickness of layer is correct by observing coating consumption and by measuring the film thickness. Recommended thickness of a layer is 0.3 mm. Level the screed with a spiked roller approx. 10 - 20 min after application. Spiked roller helps removing air bubbles from the coating.

Note! Add the remaining mixture to the next batch of the screed, do not scrape it out of the container onto the floor.

Mixing of components
       Finncoatings®color on the highest level
Mix the correct proportions of base and hardener thoroughly (approx. 2 minutes) by using a low speed hand drill with a paddle. The amount of mixture depends on the area to be coated and on the pot life of the mixture. Insufficient mixing or incorrect mixing ratio will result in uneven drying of the surface, weaken the properties of the coating and risk the success of the application.

Cleaning of tools
   
Thinner 006 1061.

EU VOC 2004/42/EC-limit value     VOC 2004/42/EC (cat A/j) 500 g/l (2010)Temafloor PU-UV: max. VOC < 500 g/l

Finncoatings® Color on the highest level

 

Finncoatings  
Heidelberger Straße 8
74858 Aglasterhausen-Germany

 

Tel. + 49 (0)6262 917095
Fax  + 49 (0)6262 917791

www.finncoatings.com
Mail. This email address is being protected from spambots. You need JavaScript enabled to view it.