TEMAFLOOR PRIMER 200

 

DESCRIPTION    
A two component solvent free epoxy varnish.

PRODUCT FEATURES
   
For priming of new and old concrete floors prior to laying Temafloor coatings and screeds. Thinned Temafloor 200 Primer penetrates well into the pores of the concrete sealing the surface and giving good adhesion for coatings and screeds. Mixed with sand also suitable for patching of concrete floors.

RECOMMENDED USES
   
Concrete floors.

TECHNICAL DATA
   Finncoatings®color on the highest level

Gloss groups    
Full-gloss

Coverage
       Finncoatings®color on the highest level

Coverage on concrete floors is on the average:
1st primer coat                     4 - 8 m2/l
2nd primer coat                  6 - 10 m2/l

 

Practical coverage depends on the porosity and evenness of the substrate and on the application method.

Thinner
       Finncoatings®color on the highest level

 

1029 and 1031

 

Mixing ratio     

 

Base 2 parts by volume 008 4400
Hardener 1 part by volume 008 4406

 

Application method        Finncoatings®color on the highest level

 

 Roller, steel or rubber trowel.
Pot-life (+23°C)     About 15 minutes after mixing, on substrate.
Drying time at 23°C and 50% relative air humidity     

Dust dry after 3 hours
Touch dry after 5 hours
Recoatable after 6 - 12 hours
Light trucking after 16 hours
Fully cured after 7 days

 
The drying times are for Temafloor 200 Primer thinned 30 % with Thinner 006 1029.

Solids volume
    Approx. 100 volume %
Density     1.1 kg / litre (mixture)

APPLICATION DETAILS

Application conditions        Finncoatings®color on the highest level
The relative humidity of the concrete should not exceed 97%. The temperature of the ambient air, surface or coating should not fall below +15ºC during application or drying. Relative humidity of air should not exceed 80%.

 

Preparation     

 

New concrete
Remove laitance by power grinding, vacuum grit blasting or hydrochloric acid etching. Choose the method best suited for the premises. After grinding remove dust carefully with a vacuum cleaner. Hydrochloric acid etching is carried out with diluted hydrochloric acid (1 part concentrated hydrochloric acid, 4 parts water). Rinse with plenty of water. Dry the floor.

Old concrete   Finncoatings®color on the highest level
Remove all grease, oil, chemicals and other impurities by MAALIPESU detergent. Remove old peeling paint layer by grinding or vacuum grit blasting. Clean out pot-holes removing all loose friable material. Open cracks with e.g. an abrasive tool. Remove loose material and dust.
Cementitious levelling screed
Check compatibility with the levelling screed manufacturer.

Priming
   

Prime using 30-50% thinned Temafloor 200 Primer epoxy varnish. Pour the varnish onto the floor and apply as much as is needed to impregnate the concrete surface. If necessary, repeat priming to get a non-porous surface. Subsequent treatment can be carried out after 2 hours using "wet-on-wet" technique.
Patching     Patch pot-holes and cracks with a mixture of unthinned Temafloor 200 Primer epoxy varnish and dry, clean sand. Mixing ratio e.g. 1 part by volume of varnish mixture and 1-2 parts by volume of sand of grain size 0.1-0.6 mm. If the topcoat will be applied as a thin layer, grind the patched areas before overcoating.
Coating     Overcoating may be carried out 6-12 hrs after priming. If the primed surface is not overcoated within 24 hrs, it should be abraded. A porous primer coat will result in holes and air bubbles in the finished coating.

Mixing of components
       Finncoatings®color on the highest level

Mix the correct proportions of base and hardener thoroughly (approx. 2 minutes) by using an industrial hand drill with a paddle. The amount of mixture depends on the area to be coated and on the pot life of the mixture. Insufficient mixing or incorrect mixing ratio will result in uneven drying of the surface, weaken the properties of the coating and risk the success of the application.

 

Cleaning of tools    

Thinner 006 1029 (or Thinner 006 1031).

 

EU VOC 2004/42/EC-limit value     VOC 2004/42/EC (cat A/j) 500 g/l (2010)Temafloor 200 Primer: max. VOC < 500 g/l

Finncoatings® Color on the highest level

 

Finncoatings  
Heidelberger Straße 8
74858 Aglasterhausen-Germany

 

Tel. + 49 (0)6262 917095
Fax  + 49 (0)6262 917791

www.finncoatings.com
Mail. This email address is being protected from spambots. You need JavaScript enabled to view it.